ANALISIS LAJU KOROSI ALUMINIUM 5083 PADA KONSENTRASI SALINITAS AIR LAUT 40 PPT UNTUK APLIKASI LAMBUNG KAPAL
Keywords:
Aluminum 5083, corrosion behavior, potentiodynamic polarization, seawater salinity, ship-hull structureAbstract
Seawater salinity was investigated as a factor affecting the electrochemical corrosion behavior of Aluminum 5083 used for ship-hull structures. Nine specimens measuring 100 × 100 × 6 mm were exposed for 14 days to salinity levels of 30, 35, and 40 ppt, with three specimens tested at each condition. Potentiodynamic polarization was conducted in a three-electrode configuration using an Autolab PGSTAT128N operated with NOVA software. Tafel analysis provided the corrosion current density (Icorr) and corrosion potential (Ecorr), while the corrosion rate was determined directly in mm/year in accordance with ASTM G102, without applying a second annualization factor. Average corrosion rates of 0.0051, 0.0169, and 0.0230 mmpy were obtained at 30, 35, and 40 ppt, respectively. Increasing salinity produced a clear rise in Icorr, whereas Ecorr varied only slightly. These results indicate that elevated salinity intensifies corrosion kinetics. The resistance classification remained Outstanding at 30–35 ppt and shifted to Excellent at 40 ppt, providing a controlled basis for salinity-sensitive inspection and corrosion protection of aluminum ship structures.References
Afandi, A., Sugiarto, S., & Rofiq, M. (2015). Korosi dan perlindungannya pada struktur baja. Universitas Brawijaya Press.
ASTM International. (2014). ASTM G5-14: Standard reference test method for making potentiostatic and potentiodynamic anodic polarization measurements. ASTM International.
ASTM International. (2023). ASTM G102-23: Standard practice for calculation of corrosion rates and related information from electrochemical measurements. ASTM International.
Dai, Z., Xiao, Z., Zhao, D., Xiao, S., Huang, Y., & Dai, Q. (2024). Multi-scale study on the electrochemical behavior and corrosion mechanism of 5083 aluminum alloy with different microstructures in a NaCl environment. Physical Chemistry Chemical Physics, 26, 28662–28679. https://doi.org/10.1039/D4CP03380A
Deng, C.-M., Liu, Z., Xia, D.-H., Behnamian, Y., & Hu, W. (2024). On the localized corrosion of AA5083 in a simulated dynamic seawater/air interface—Part 3: Effects of sensitization. Corrosion Science, 228, 111821. https://doi.org/10.1016/j.corsci.2024.111821
Deng, C.-M., Xia, D.-H., Zhang, R., Behnamian, Y., Hu, W., & Birbilis, N. (2023). On the localized corrosion of AA5083 in a simulated dynamic seawater/air interface—Part 2: Effects of wetting time. Corrosion Science, 221, 111367. https://doi.org/10.1016/j.corsci.2023.111367
Gao, Y., Feng, D., Moradi, M., Yang, C., Jin, Y., Liu, D., Xu, D., Chen, X., & Wang, F. (2021). Inhibiting corrosion of aluminum alloy 5083 through Vibrio species biofilm. Corrosion Science, 180, 109188. https://doi.org/10.1016/j.corsci.2020.109188
Ji, Y., Mao, Y., Dang, L., Xia, D.-H., & Hu, W. (2023). A high-resolution characterisation of localised corrosion of AA5083-H111 in simulated seawater by TEM. Corrosion Engineering, Science and Technology, 58(3), 223–229. https://doi.org/10.1080/1478422X.2022.2162662
Marques, M. J. F., Benedetti, A., Castelli, F., Delucchi, M., Faimali, M., Delsante, S., Valenza, F., Garaventa, F., Pavanello, G., & Basseguy, R. (2023). Influence of natural seawater variables on the corrosion behaviour of aluminium-magnesium alloy. Bioelectrochemistry, 149, 108321. https://doi.org/10.1016/j.bioelechem.2022.108321
Xia, D.-H., Ji, Y., Zhang, R., Mao, Y., Behnamian, Y., Hu, W., & Birbilis, N. (2023). On the localized corrosion of AA5083 in a simulated dynamic seawater/air interface—Part 1: Corrosion initiation mechanism. Corrosion Science, 213, 110985. https://doi.org/10.1016/j.corsci.2023.110985